Recycling of waste cotton fabrics into biodegradable antimicrobial packaging materials
Zhou, Chufan · container not stated · 2021
Not cached yet. This record was fetched live for this request and is stored after the lookup. Reopening the page should serve the cached copy.
· OpenAlex · dissertation · 2021
Abstract
Today, there is a concern about the rapid increase in waste textile. Traditional treatments (such as landfill and incineration) have resulted in numerous disposal, utilization and management issues. Cotton is one of the most utilized fibers in textile industry, which consists of over 90% of cellulose. Thus, waste cotton fabrics could be a useful resource of cellulosic materials. In this study, the recycling of waste cotton fabrics into biodegradable packaging materials by dissolution and regeneration was investigated, and mechano-bactericidal packaging was developed from the regenerated cellulose films and cellulose nanocrystals (CNCs).
In Chapter 2, the recent research on biomass waste utilization and biomass wastes derived functional materials was reviewed, which mainly focused on the following three aspects: (1) extraction of natural polymers from biomass wastes, (2) reuse of biomass wastes, and (3) preparation of carbon-based materials as novel adsorbents, catalyst carriers, electrode materials, and functional composites. In Chapter 3, the formation of natural and synthetic nanopillared surfaces was summarized, and the mechanism of action and the factors that influence their mechano-bactericidal activities were highlighted.
In Chapter 4, the dissolution of three typical waste cotton fabrics (t-shirts, bed sheets and jeans) in NaOH/urea aqueous solution, H2SO4 aqueous solution, and LiCl/DMAc solution was investigated. Compared to different types of cotton fabrics, the effects of three solvents on the dissolution of fabrics were more obvious, leading to the significant changes in the structure and properties of regenerated cellulose films.
Cotton fabrics (about 2-5%) were rapidly dissolved (8 min) in H2SO4 and NaOH/urea solvents after acid pretreatment, while the dissolution in LiCl/DMAc solvent did not need any pretreatment, but a lower cellulose concentration (1%), higher dissolution temperature (80 °C), and longer dissolution time (24 h) were required. The films produced from bed sheets in NaOH/urea solution exhibited the highest tensile strength, thermal stability, and water vapor barrier property. It was because of the stronger cellulose chain entanglement and hydrogen bonds induced by the higher cellulose concentration in NaOH/urea solution.
In Chapter 5, a new strategy namely mechano-bactericidal effect inspired by the naturally occurring surfaces was applied to construct antibacterial films from waste cotton fabrics. Various amounts of CNCs were deposited on the surface of regenerated cellulose films. The results revealed that the all-cellulose films displayed an obvious and fast bactericidal activity against both Gram-negative (Escherichia coli) and Gram-positive (Listeria monocytogenes) bacteria within 3 min contact. The increase of CNC contents from 3% to 10% slightly improved the bactericidal activity, but the extension of contacting time (up to 2 h) did not affect the log reduction of bacteria.
In addition, the surface coating with CNCs significantly enhanced the tensile strength and Young’s modulus of regenerated cellulose films from 71.31±6.10 to 131.44±3.83 MPa and from 3051.39±87.81 to 5704.33±392.32 MPa, respectively. Overall, this research proves the feasibility to recycle waste cotton fabrics into biodegradable cellulose films, which can be potentially used in various food and agricultural applications. It also provides great prospects for the development of new generation of antibacterial packaging films