Nobel Metal Nanoparticles in Bio-LED
Yen‐Hsun Su, Sheng-Lung Tu, Wei-Min Zhang · InTech eBooks · 2012
Not cached yet. This record was fetched live for this request and is stored after the lookup. Reopening the page should serve the cached copy.
InTech eBooks · OpenAlex · book-chapter · 2012
Abstract
Nanomaterials are well known for their interesting physical chemical properties [1][2][3][4][5][6][7].Recently, noble metal nanoparticles have attracted attention [9][10][11][12][13][14][15] due to their optical property of surface plasmon resonance.Surface plasmon resonance produces hot light spots due to a stronger electromagnetic field.Because of their low toxicity, ease of delivery, and strong and tunable surface plasmon resonance, noble metal nanoparticles are used in the field of the photothermal ablation therapy to treat cancer [10].Plants help people confront the global warming by absorbing CO 2 in the photosynthesis process.If plants were able to do the photosynthesis process day and night, absorbing CO 2 will act in day and night.In this paper, we investigate the life time of noble metal nanoparticle colloids on plants specifically.The buds of Floppers, Bryophyllum pinnatum (Lam.)Kurz., are watered the noble metal cluster colloids.The buds are recorded for six weeks.The results show that noble metal nanoparticle colloids exit plant growth, with the Pt nanoparticles aggregating on the leaf.We expect that this research has potential applications in the fields of biosensing, bio-LED, bioimaging, nanophotonics, photothermal ablation therapy, and nanotoxicity.
Experimental produreChemicals and materials.We prepared 10 L standard solution by adding MgCl= 10.0 ppm, KCl=0.5 ppm, NaCl= 8 ppm, and FeCl 3 = 0.04 ppm in Milli-Q water.Trisodium citrate (99%) and HAuCl 4 , AgNO 3 , and H 2 PtCl 6 were purchased from Showa Chemical Co.(Tokyo, Japan) and Alfa Aesar Chemical Co.(Lancashire, England) and used as supplied, respectively.Milli-Q water was obtained from the Milli-Q Element system (Massachusetts, USA), which employs ultra-clean materials and a succession of optimized water purification technologies to produce 18.2 MΩ/cm resistivity ultrapure water (at 25 °C), ideal for trace analysis methods.The solution used in this work was freshly prepared and deoxygenated by bubbling nitrogen gas for at least 30 min prior to use.All materials and apparatus were sterile.Preparation of noble nanoparticles.Au NPs were prepared by a chemical-reduction method with Au, Pt, Ag-salt and Na-cit standard solutions.1.5 ml of freshly prepared 0.34 M trisodium citrate (aq) solution was added to 15 ml of 0.5 mM HAuCl 4(aq) solution, AgNO 3(aq) www.intechopen.com
Open the resolved locator · 10.5772/33503