MEACTOS environmentally-assisted crack initiation data for constant extension rate tensile tests in BWR/NWC environment on cold-worked 316L stainless steel
Ritter, S. Et Al., PSI-Paul Scherrer Institute · ODIN: Online Data & Information Network for Energy · 2024
Not cached yet. This record was fetched live for this request and is stored after the lookup. Reopening the page should serve the cached copy.
ODIN: Online Data & Information Network for Energy · OpenAlex · dataset · 2024
Abstract
Data collection created at PSI, ZAG, RATEN ICN, and EC JRC in the scope of the H2020 MEACTOS project investigating the mitigation of environmentally-assisted cracking through optimisation of surface condition. The work was concerned with SSRT/CERT accelerated tests on flat tapered tensile specimens in BWR/NWC environment to determine the stress corrosion cracking threshold stress. The material investigated was cold-worked 316L stainless steel.
Open the resolved locator · 10.5290/68
Metadata licence: OpenAlex metadata (CC0)