Chemical durability of sintered glass-composite prepared from glass cullet and waste foundry sand
Veljko Savić, Vladimir S. Topalović, Srdjan D. Matijašević, Jelena D. Nikolić, Snežana Grujić, Snežana Zildžović, Aleksandra M. Radulović · Metallurgical and Materials Engineering · 2020
Not cached yet. This record was fetched live for this request and is stored after the lookup. Reopening the page should serve the cached copy.
Metallurgical and Materials Engineering · Association of Metallurgical Engineers of Serbia · article · 2020
Abstract
In this study, the glass-composite was prepared using glass cullet and waste foundry sand as raw materials. The powder technology route was employed. The mixtures containing 10-50 wt% of the sand were sintered at T = 750 °C for t =1h. XRD and DTA analyses were performed. The chemical durability of the resulting glass-composite was determined by leaching test in HCl, H2SO4, NaOH and distilled water at T = 95 °C for t =1h. It was shown that the sintering process carried out without the crystallization of the glass matrix. The lowest chemical durability was determined in alkali solution of glass-composite.
Open the resolved locator · 10.30544/477
Metadata licence: OpenAlex metadata (CC0)