Residual stresses in weld overlay tubes: A finite element study

TN (United States) Oak Ridge National Lab., B Taljat, USDOE Assistant Secretary for Energy Efficiency and Renewable Energy, Washington, DC (United States), T Zacharia, X Wang, J Keiser, Z Feng, Michael J. Jirinec · OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · 1997

  • DOI 10.2172/486147
  • Publisher Office of Scientific and Technical Information
  • Type report
  • Issued 1997

Not cached yet. This record was fetched live for this request and is stored after the lookup. Reopening the page should serve the cached copy.

OSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information) · Office of Scientific and Technical Information · report · 1997

Abstract

Residual stresses and strains in a tube with circumferential weld overlay were analyzed by the finite element (FE) method. The objective of this work was to develop and verify a FE model, to determine the magnitude and distribution of residual stresses in the weld overlay tube, and to evaluate the significance of two contributing factors to residual stress: (1) difference in material properties between tube and weld material, and (2) thermal gradients in the weld. An axisymmetric FE model was developed to simulate the circumferential two-layer welding process of alloy 625 overlay on SA210 tube.

The first layer was modeled as a gas metal arc welding process with filler metal, whereas the autogenous gas tungsten arc welding process was modeled for the second layer. Neutron diffraction technique was used to experimentally determine residual elastic strains in the weld overlay tube. Comparison with the FE results shows overall good agreement. Both the experimental and FE results show high compressive stresses at the inside tube surface and high tensile stresses in the weld overlay.

This suggests that weld overlay may be used to relieve tensile or produce compressive stresses at the inside tube surface, which is significant for applications where crack initiation is found at the root pass of the joining weld.

Open the resolved locator · 10.2172/486147

Metadata licence: OpenAlex metadata (CC0)

Registry
OpenAlex DOI index + API
Fetched
2026-11-20 14:15 UTC
Cache state
not cached yet (bulk-index+openalex)
Locator
https://www.osti.gov/biblio/486147
Metadata licence
OpenAlex metadata (CC0)
Scope
Metadata as returned by the resolver; abstracts are never generated here.